                              | Qualified by Laser Interferometer Gravitational-Wave Observatory for Optical Assembly Applications |  
                              |  |  
                              | Ultra low outgassing epoxy Master Bond EP30-2 was utilized by Laser Interferometer Gravitational-Wave Observatory (LIGO) in their bonding of optical components to prove Einstein’s 1915 general theory of relativity – 100 years after it was predicted! The main applications involved bonding prism elements, and bonding acoustical dampeners to optical components.  See how they successfully used the EP30-2 epoxy compound. |  
                              |  |  
                              |  |  |  
                        |  |  |  |  
            |  |  |  
    
      |  |  
      | 
          
            |  |  
            | 
 
                