Master Bond Adhesives, Sealants and Coatings Offer Superior Resistance To Vibration, Impact and Shock
Master Bond Inc. has developed a wide range of bonding, sealing and coating
formulations specifically designed to resist exposure to vibration,
impact and shock. These compounds consist of epoxy, silicone,
polyurethane, polysulfide and UV cure systems. The have excellent
adhesion to similar and dissimilar substrates, including metals, ceramics,
glass, rubbers and most plastics. They are noted for providing improved
durability, high peal/shear strength properties and the ability to withstand
thermal cycling.
Our vibration, impact and shock resistant compounds are successfully employed in the aerospace, automotive, electronic, optical, electrical, medical and oil/chemical processing industries. They are used in applications ranging from design and production to repair/maintenance to field service. Specific grades offer:
Electrical and Thermal Conductivity
- Superior Electrical Insulation Properties
- High/Low (Cryogenic) Temperature Serviceability
- Low Shrinkage
- Resistance to Water and Many Chemicals
- Optical Clarity
- Abrasion Resistance
- Fast Curing
- Gap-Filling
- Easy Application
Contact our world class technical staff today,
and let them recommend a Master Bond product specifically for
your application.
Our Most Popular
Vibration,
Shock & Impact Resistant Systems...
| Product |
Description |
EP21TDC-2 |
Two part room temperature curing
epoxy with excellent flexibility (elongation over 150%)
and ability to withstand mechanical shock, vibration
and impact. Resistants thermal cycling. |
SUPREME 10HTFL |
One part oven cured epoxy (250-300°F)
with superior bonding and sealing properties. Withstands
heavy mechanical shock, impact and vibration. Serviceable
from 4K to +350°F. Outstanding peel strength >50pli. |
UV15X-5 |
One part UV curable adhesive/sealant
with rapid cure. Outstanding abrasion resistance. Superior
electrical insulation properties. Highly flexible
and resists vibration, shock and impact. |
Packaged the Way You Need
It
 |
 |
We offer a wide array of packaging
options to speed productivity, minimize waste and save energy
including...
• Quantities from grams to gallons
• Cans, bottles
and jars • Cartridges for manual and pneumatic guns
• Premixed and frozen
syringes
• Bipaks for field service kits
|
High Reliability & Performance
|
|