MASTER BOND ANAEROBIC APPLICATION SELECTOR GUIDE

Anaerobic Systems for Retaining & Sealing Bolts, Nuts, Screws, Studs, Bearings, Bushings, Seals, Keys & Splines.

INDUSTRIAL GRADES

Master
Bond
Grade

Locking Torque
3/8” Bolts,

In - #’s


Viscosity
CP


Color
Code


Cure
Time



Typical Gap Filled


Service Temp Range, °F

Applications

GP2

130

20,000+
thixotropic

Red

greater than
2 hours

0.020”

-65 to +350

“no drip”; strong; locking, bonding and sealing; seal vertical flanges.

GP22

55

20,000+
thixotropic

Red

greater than
2 hours

0.020”

-65 to +350

“no drip”; medium strength; locking, bonding and sealing; pipe sealant.

GP222

30

20,000+
thixotropic

Red

greater than
2 hours

0.020”

-65 to +350

“no drip”; for quick disassembly; for locking, bonding and sealing.

GP122

40

900

Purple

greater than
2 hours

0.010”

-65 to +350

mild strength; locking, bonding and sealing; for ready disassembly.

GP144

80

1,100

Blue

less than
1 hours

0.012”

-65 to +350

medium strength; locking, bonding and sealing; retaining bearings, bushings.

GP166

190

1,500

Red

1 - 2
hours

0.012”

-65 to +350

high strength; locking, bonding and sealing; retaining bearings, seals, bushings

GP555

210

700

Red

1 - 2
hours

0.010”

-65 to +350

locking and retaining studs, nuts, screws; sleeves, bushings and cylindrical parts retained.

GP575

220

7,000

Red

1 - 2
hours

0.015”

-65 to +350

high strength cures for larger clearances; seal flanged assemblies.

GP595

245

20

Green

less than
1 hours

0.005”

-65 to +350

very fast high strength cures, wicking grade, also a weld sealant.

GP666

284

125

Green

less than
1 hours

0.005”

-65 to +350

retaining compound; locking, sealing and bonding assemblies.

GP55

210

550

Green

greater than
2 hours

0.010”

-65 to +350

retaining bearings, shafts and hubs; good temperature resistance.

GP50

295

2,000

Green

greater than
2 hours

0.015”

-65 to +350

high strength retaining compound, permanent assemblies.

Strengths and cure time measured with unprimed clean 3/8 - 24 carbon steel fasteners.

Strengths reported after 24 hour cure at room temperature in accordance with MIL-S-22473D.

Master Bond Inc.

Adhesives, Sealants & Coatings • 154 Hobart Street • Hackensack, N.J.  07601 • Tel: 201-343-8983 • Fax: 201-343-2132

Notice:  Master Bond believes the information on the data sheets is reliable and accurate as is technical advice provided by the company.  Master Bond makes no warranties (expressed or implied) regarding the accuracy of the information and assumes no liability regarding the handling and usage of this product.                                                                                                                                                     D019


MASTER BOND ANAEROBIC APPLICATION SELECTOR GUIDE

Anaerobic Systems for Retaining & Sealing Bolts, Nuts, Screws, Studs, Bearings, Bushings, Seals, Keys & Splines.

MIL-S-22473D GRADE EQUIVALENTS

Master
Bond
Grade

MIL
Equivalent
Grade

Locking Torque
3/8” Bolts,

In - #’s


Viscosity
CP


Color
Code


Cure
Time



Typical Gap Filled


Service Temp Range, °F

Applications

GP6

AV

210

200

Red

1 - 2
hours

0.010”

-65 to +350

standard grade, durable thread locking, bonding and sealing.

GP66

AA

284

20

Green

1 - 2
hours

0.005”

-65 to +350

high strength cures, retaining parts, subjected to various loads, fine threads.

GP4

A

245

20

Red

less than
1 hours

0.005”

-65 to +350

very fast high strength cures, also wicking grade.

GP333

AVV

240

4000

Red

greater than
2 hours

0.015”

-65 to +350

very high strength cures, coarser threads, worn parts.

GP8

B

150

180

Yellow

1 - 2
hours

0.005”

-65 to +350

medium strength cures, fine threads, small clearances.

GP10

CV

55

200

Blue

greater than
2 hours

0.010”

-65 to +350

low strength cures, hydraulic sealant, coarser threads.

GP12

C

50

20

Blue

greater than
2 hours

0.005”

-65 to +350

for fast disassembly, fine threads, small clearances

GP14

CVV

55

8000

Blue

greater than
2 hours

0.015”

-65 to +350

for fast disassembly, coarser threads, larger clearances.

GP16

H

22

200

Brown

greater than
2 hours

0.005”

-65 to +350

very low strength for easy disassembly, fine threads, small clearances.

GP18

HV

20

220

Brown

greater than
2 hours

0.010”

-65 to +350

very low strength for easy disassembly, coarser threads, larger clearances.

GP20

HVV

17

8500

Brown

greater than
2 hours

0.015”

-65 to +350

very low strength for easy disassembly, coarse threads, large clearances.

GP25

E

40

20

Purple

greater than
2 hours

0.005”

-65 to +350

low strength cures, fine threads, small clearances.

GP27

EV

40

200

Purple

greater than
2 hours

0.010”

-65 to +350

low strength cures, coarser threads, larger clearances.

Strengths and cure time measured with unprimed clean 3/8 - 24 carbon steel fasteners.

Strengths reported after 24 hour cure at room temperature in accordance with MIL-S-22473D.

Master Bond Inc.

Adhesives, Sealants & Coatings • 154 Hobart Street • Hackensack, N.J.  07601 • Tel: 201-343-8983 • Fax: 201-343-2132

Notice:  Master Bond believes the information on the data sheets is reliable and accurate as is technical advice provided by the company.  Master Bond makes no warranties (expressed or implied) regarding the accuracy of the information and assumes no liability regarding the handling and usage of this product.                                                                                                                                                     D019