The following is a news release from Master Bond Inc. You have received it  because you are listed as an editor for your publication.
  Attached to this email is a low resolution version of the photograph that is  included in the press kit for this product.
  A high resolution version of this image and files with the body text of this  release in Word, HTML and text formats are available at https://www.masterbond.com/newsrelease/ep21arhtnd-2. 
  -----------------------------------------------------------------
Master Bond EP21ARHTND-2 is a two part epoxy adhesive, designed to withstand prolonged exposure to a wide range of chemicals. “The system’s chemical resistance was successfully tested in chemicals such as 98% sulfuric acid, 25% hydrochloric acid, 20% phosphoric acid, and 15% nitric acid, by soaking cured samples for more than 12 months”, says Senior Product Engineer Rohit Ramnath. “The product also passes the damp heat reliability testing by withstanding 1000 hours of 85°C and 85% Relative Humidity (RH).”
Although EP21ARHTND-2 is capable of curing at room temperature, to optimize its acid resistance properties, a cure schedule of overnight at ambient temperatures, followed by a heat cure of 150-200°F for 2-4 hours or longer is typically recommended. It is a reliable electrical insulator with a volume resistivity greater than 1014 ohm-cm at 75°F, and dielectric strength of 440 volts/mil at 75°F for a 1/8-inch test specimen. Other noteworthy properties include a tensile strength of 9,000-10,000 psi, and a Shore D hardness of 75-85. The adhesive provides good heat resistance and is serviceable from -60°F to +400°F.
EP21ARHTND-2 does not contain solvents and is RoHS compliant. The product bonds well to metals, ceramics, composites, rubbers and plastics. It features a smooth paste-like consistency and will not flow, or sag once applied, making it ideal for bonding and sealing applications. It is available for use in ½ pint, pint, quart and gallon container kits. Specialty packaging can also be provided in 50 ml (cc) double barrel cartridges, which not only eliminates the need for manual measuring as well as mixing, but also enables the possibility of manual or automated dispensing.
Master Bond's chemically resistant systems provide protection against a wide variety of chemicals, including acids, bases, solvents, water, alcohol and sterilants. These compounds are utilized in chemical processing plants, chemical piping and tanks, medical devices, aerospace and many other industries and applications. Master Bond custom formulated systems are tailored to meet specific requirements. Read more about Master Bond’s chemically resistant adhesives at https://www.masterbond.com/properties/chemical-resistance or contact technical support to discuss your application.
TECH SUPPORT
Email: technical@masterbond.com
Web: https://www.masterbond.com/contact 
Tel: +1-201-343-8983
Note to Editors:
For a full product description, please visit: https://www.masterbond.com/tds/ep21arhtnd-2
  Check out new videos on our YouTube channel: https://www.youtube.com/user/MasterBondVideo
 
You can embed any of our videos on your website.
CONTACT
  James Brenner, Marketing Manager
  Email: jbrenner@masterbond.com
  Tel: +1-201-343-8983
  Fax: +1-201-343-2132
MASTER BOND INC.
  154 Hobart Street 
  Hackensack,   NJ 07601-3922 
  Web: www.masterbond.com
# # #