Go to the MasterBond.com home page
Master Bond Polymer System EP13 Product Description

 

MASTER BOND POLYMER SYSTEM EP13
One Component, Heat Curing Structural Adhesive Featuring High Tensile Shear Strength and
High Temperature Resistance for Optimal Bonding Performance Up To 450°F

Master Bond Polymer System EP13 is a one component heat curing epoxy featuring high shear strength and very high temperature resistance. This one component system is formulated to cure at temperatures from 300°F to 350°F for 60-90 minutes. Upon cure, EP13 readily attains tensile shear strengths in excess of 3,500 psi. The service temperature range is -60°F to 450°F. EP13 forms rigid and dimensionally stable bonds with minimal shrinkage upon cure. It is 100% reactive and does not contain any solvents or diluents. EP13 is a paste and can be applied to vertical surfaces without sagging or dripping. Also, EP13 possesses high compressive strength and is readily machinable.

As a one part system, Master Bond Polymer System EP13 is easy to handle as it does not require mixing prior to use and has an unlimited working life at room temperature. It bonds well to a wide variety of substrates including metals, glass, ceramics, vulcanized rubbers and many plastics. It has excellent resistance to a wide range of chemicals including fuels, acids, bases, oils and many solvents. The standard color is gray. EP13 is an excellent electrical insulator. The cured adhesive fully meets the requirements of MIL-MMM-A-132.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2009 Master Bond Inc., All Rights Reserved