Master Bond Polymer System EP21BAS is a radioopaque two component epoxy compound which cures readily at ambient or more quickly at elevated temperatures. This epoxy polymer system features outstanding physical and chemical properties. A user friendly one-to-one (1/1) mix ratio by weight or volume facilitates processing. Additionally, EP21BAS has the unusual characteristic of being able to adjust the properties of the cured system by altering the mix ratio. Adding more part "A" (e.g. 2:1 mix ratio) gives a more rigid cure while adding more part "B" (e.g. 2:3 mix ratio) gives a more forgiving cure. EP21BAS produces high strength, durable bonds, seals, coatings and castings which hold up well to thermal cycling and resist many chemicals including water, oils, fuels, acids, bases and salts. It is serviceable over the wide temperature range of -60°F to +250°F. It adheres well to a variety of substrates including metals, glass, ceramics, wood, rubber, and many plastics. Once cured, EP21BAS is an excellent electrical insulator. This exceptionally versatile system is widely used in the electronic, electrical, optoelectronic and medical device industries. The cured polymer compound fully meets the requirements for radioopacity needed in medical devices and similar applications. While the standard color of the cured material is an off-white, a wide variety of additional color choices are also available.
|