EP21TDCS-LO Product Description

Two Component Silver Conductive Epoxy for High Performance Bonding and Sealing Featuring High Peel Strength, Superior Toughness and Exceptionally Low Volume Resistivity. Passes ASTM 595 for NASA Low Outgassing

Master Bond Polymer System EP21TDCS-LO is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated temperatures. Unlike the majority of two part silver conductive epoxy systems, the EP21TDCS-LO has a one-to-one mix ratio by weight or volume. It readily develops a high bonding strength of more than 1,800 psi tensile shear and a T-peel strength of greater than 20 pli when measured and cured at 75°F. It is 100% reactive and does not contain any diluents or solvents. The volume resistivity of the cured system is less than 10-3 ohm-cm.

Master Bond Polymer System EP21TDCS-LO can be applied with minimal sagging or dripping even on vertical surfaces. The high strength bonds are remarkably adaptable to thermal cycling and resistant to chemicals including water, oil and most organic solvents. The EP21TDCS-LO system operates over the exceptionally wide temperature range of 4K to +275°F enabling it to be serviceable even in cryogenic applications. Adhesion to metals, glass, ceramics, vulcanized rubbers and many plastics is excellent. Parts A and B are both colored silver. Master Bond EP21TDCS-LO adhesive is widely used in the electronic, electrical, computer, semiconductor, microwave and appliance and industries, among others.

LATEST PRODUCT

Offering a unique blend of high performance properties, Master Bond MasterSil 153 is often used in a...

LATEST WHITE PAPER

Selecting the right adhesive is a balancing act as engineers attempt to find products that meet conflicting end-use and...