Master Bond Polymer Adhesive EP23 is a mineral filled two component epoxy adhesive for high performance bonding formulated to cure at room temperature or more rapidly at elevated temperature with a one-to-one mix ratio, weight or volume. The EP23 adhesive develops high bonding strength of more than 2200 psi at room temperature which unlike that of many other epoxy adhesives, is relatively insensitive to mixing ratio or substrate cleaning procedures. Master Bond Polymer Adhesive EP23 produces durable and tough high strength bonds with outstanding adhesion to metals especially steel, iron and aluminum; ceramics; glass; wood; vulcanized rubber; and many plastics. The bonds feature remarkably high resistance to thermal cycling and chemicals including water, oil and most organic solvents, over the exceptionally wide temperature range of -60°F to more than 250°F. Color of part A tan, part B opaque tan. Master Bond EP23 adhesive is widely used in the electronic, electrical, computer, construction, metalworking, appliance, automotive and chemical industries.
|