Master Bond Polymer System EP30-2 is
a low viscosity, two component epoxy resin compound for high performance
bonding, laminating and sealing formulated to cure at room temperature
or more rapidly at elevated temperatures with a 100/10 mix ratio by weight.
This resin system is 100% reactive and does not contain any solvents or
other volatiles. It is especially recommended where low viscosity is required
for ease of application and and applications in which bonded assemblies
must exhibit superior dimensional stability. Shrinkage upon cure is exceptionally
low - 0.0003 incheses/inch.
Master Bond Polymer System EP30-2 produces high strength and tough bonds
which are remarkably resistant to thermal cycling and chemicals including water,
oil and most organic solvents, over the exceptionally wide temperature range
of -60°F to has high as 300°F.
Adhesion to both similar and dissimilar materials including metals, glass,
ceramics, wood, vulcanized rubbers and many plastics is excellent. The hardened
resin is an electrical insulator. Color of parts A and B is clear. Master
Bond Polymer System EP30-2 is widely used in the electronic, electrical, computer,
construction, metalworking, appliance, automotive and chemical industries.