Go to the MasterBond.com home page
Master Bond Polymer System EP30F Product Description

 

MASTER BOND POLYMER SYSTEM EP30F
New Fast Curing Liquid Epoxy Resin System for High Pertormance
Abrasion and Chemical Resistant Seamless Floors

Master Bond Polymer System EP30F is a new fast curing liquid epoxy resin compound for high perform-ance abrasion and chemical resistant seamless floors. This easy-to-use two component epoxy resin system offers a uniquely attractive combination of application and performance properties including substantially faster installations with significantly lower labor costs, durable high performance even under exceptionally heavy traffic conditions and remarkably low maintenance. Master Bond Polymer System EP30F is comprised of two components, the resin and the hardener. They can be easily mixed and then applied onto most any properly prepared clean and sound surface forming virtually inseparable bonds to concrete, wood, metal, tile etc. Surface texture of this remarkably cost effective long-life epoxy resurfacing can be non-skid as required or it can be finished to have a smooth finish. Cracks and other surface imperfections are completely and permanently filled.

Master Bond Polymer System EP30F is particularly recommended for all kinds of industrial, commercial and institutional floors especially in areas where a high degree of durability, abrasion and chemical resistance, dimensional stability, easy maintenance and good sanitation are needed. It has been used with remarkable success in factories, warehouses, chemical plants, dairies, breweries, bakeries, hotel and hospital kitchens, cafeterias, shower and locker rooms, offices, corridors, high-rise construction, airports and other public build-ings, patios, swimming pools and show rooms.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2008 Master Bond Inc., All Rights Reserved