Master Bond Polymer System EP30HV Product Description

 

MASTER BOND POLYMER SYSTEM EP30HV
Two Component, Room Temperature Curing Epoxy System for High Performance Bonding, Sealing, Coating and Casting Featuring Excellent Physical Strength Properties and Optical Clarity
Meets FDA Chapter 1, Sections 175.105 & 175.300 for Food Applications

Master Bond Polymer System EP30HV is a low viscosity, two component epoxy system for high performance bonding, sealing, coating and casting. It is formulated to cure at room temperature or more rapidly at elevated temperatures. It has an easy to use, non-critical 4 to 1 mix ratio by weight. This system is 100% reactive and does not contain any solvents or other volatiles. It is especially recommended when low viscosity, excellent physical strength properties along with optical clarity are required. The linear shrinkage after cure is exceptionally low, about 0.0003 inches/inch. The combination of superb physical properties and convenient processing enable EP30HV to be used not only for bonding and coating, but also for potting and encapsulation, especially of electronic or optical assemblies.

Master Bond Polymer System EP30HV produces high strength, rigid bonds which are remarkably resistant to chemicals including water, oils, acids, bases and many organic solvents. The temperature range is -60°F to 300°F. It adheres well to a wide variety of materials including metals, glass, ceramics, wood, rubbers and many plastics. The cured epoxy has excellent electrical and thermal insulation properties along with outstanding light transmittance from 350 to about 2400nm. Master Bond Polymer System EP30HV is widely used in the electronic, electrical, computer, aerospace, optical, fiber optic, medical, automotive and chemical industries.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2008 Master Bond Inc., All Rights Reserved