Master Bond Polymer System EP30M3LV-2 is a low viscosity, two component epoxy compound for high performance, chemical resistant casting and potting applications, formulated to cure at ambient temperatures or more rapidly at elevated temperatures, with a convenient two (2) to one (1) mix ratio. This compound is 100% reactive and does not contain any solvents or other volatiles. It contains a special air release agent. Master Bond Polymer System EP30M3LV-2 is particularly recommended where a low viscosity is required and cured castings must withstand severe environmental conditions such as exposure to various chemicals and temperature cycling up to 275°F. Adhesion to both similar and dissimilar substrates is excellent. The hardened material is an electrical insulator. Color of part A is black; part B is amber. Master Bond Polymer System EP30M3LV-2 is widely used in the electronic, electrical, computer, construction, appliance, metalworking, automotive and chemical industries.
|