Master Bond Polymer System EP39-2 Product Description

 

MASTER BOND POLYMER SYSTEM EP39-2
Low Viscosity, Fast Curing, Two High Performance Optical Epoxy For Bonding, Sealing,
Coating & Casting Featuring Excellent Chemical Resistance

Master Bond Polymer System EP39-2 is a fast curing, low viscosity, optically clear two component epoxy system for high performance bonding, sealing, coating and casting. It is 100% reactive and does not contain any diluents, solvents or other volatiles. The mix ratio is a convenient 2 to 1 by weight. EP39-2 is very fast curing, even in very thing sections. Films as thin as 5 mil become tack free at ambient temperatures in only 3 hours and fully cure in 6-10 hours. The aforementioned film will even become tack-free at 40°F within 9 hours. Other desirable characteristics include resistance to blushing and exudation, good electrical insulation properties, high toughness, superior wear resistance and outstanding chemical resistance (see chart below). Service temperature range is -60°F to 300°F.

Master Bond Polymer System EP39-2 is en exceptionally versatile system. Its marvelous optical clarity and light transmission properties make it an excellent candidate for many optical and fiber-optic applications including bonding, sealing, coating and casting. EP39-2 bonds well to a wide variety of substrates including most metals, glass and plastics and is easy to apply by roller, brush or conventional spray equipment.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2008 Master Bond Inc., All Rights Reserved