Master Bond Polymer System EP39-3CLV is a low viscosity, clear, two component epoxy resin system for high performance flooring with exceptional solvent and acid resistance. It is formulated to cure quickly at ambient temperatures with a convenient five (5) to one (1) mix ratio by weight. This compound is 100% reactive and does not contain any solvents or diluents. Cure is exceptionally fast-thin films (12-16 mils) become tack-free in only 2-2t/2 hours at ambient temperatures. Master Bond Polymer System EP39-3CLV conforms to section 175.300 of the Federal Register and can be used in applications involving direct contact with foods. The ready cure characteristics, inherent toughness and high chemical resistance of this epoxy resin system have proven particularly attractive for applications where new floors must be put into service in a matter of hours and then perform well over many years of service in contact with organic solvents, acids and many other chemicals.
Master Bond Polymer System EP39-3CLV has proven ideaily suited for industrial as well as institutional and commercial flooring applications particularly in locations requiring durability, chemical resistance, easy low cost maintenance and a high degree of sanitation. It is highly recommended for commercial areas such as shopping centers, offices, showrooms, corridors, hotels and motels, patios, swimming pool decks, classrooms, and industrial locations including factories, warehouses, food processing plants, dairies, meat preparation facilities, commercial kitchens, pharmaceutical plants, computer installations and chemical plants. Excellent for new construction, restoration and repair.
|