Master Bond Polymer System EP3HT is a one component system featuring high shear strength, good temperature resistance along with a fast cure schedule. Typical curing schedules are 5-10 minutes at 300°F or 20-30 minutes at 250°F (minimum cure temperature is 235°F-240°F). Tensile shear strengths in excess of 2,100 psi are readily obtained after these fast cure times. EP3HT requires no mixing prior to use and has unlimited working life at room temperature. The service temperature range is -60°F to 400°F. It is 100% reactive and does not contain any solvents or volatiles. A non-drip version called EP3HTND-2 which can be applied to vertical surfaces without sagging or dripping is also available.
Master Bond Polymer System EP3HT produces durable, high strength bonds which are remarkably resistant to severe thermal cycling and many chemicals including water, oil, fuels and most organic solvents even upon prolonged exposures. Adhesion to metals, glass, ceramics, vulcanized rubbers and many plastics is excellent. The cured adhesive/sealant is a superior thermal and electrical insulator. Its color is yellow to brown, although other colors are also available. The convenient handing and rapid cure speed of EP3HT makes it ideally suited for demanding manufacturing applications. The cured adhesive fully meets the requirements of MIL-MMM-A-132
|