Master Bond Polymer System EP41S Med Product Description

 

MASTER BOND POLYMER SYSTEM EP41S MED

Two Component Low Viscosity Epoxy System For High Performance
Bonding, Sealing, Coating. Including Small Encapsulations, Pottings & Castings Featuring Fast Set-Up and Handling Time.

Meets USP Class VI Specifications for Medical Applications.  Conforms Title 21, U.S. Code of
Federal Regulations, FDA Chapter 1, Section 175.105 & 175.300 for Food Applications.

Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings. It is formulated to cure readily at room temperature or more quickly at elevated temperatures. One notable property is its very fast curing at room temperature.  It has a 5 to 1 mix ratio by weight and contains no solvents or diluents.  Master Bond Polymer System EP41S Medical produces high strength rigid bonds, which are remarkably resistant to chemicals including water, oil, many organic solvents, as well as cold sterilants, ETO and gamma radiation.  It has a wide service temperature range of -60°F to + 250°F.  It bonds well to a wide variety of substrates including metals, glass, ceramics, wood and many plastics.  EP41S Medical has exceptionally low linear shrinkage upon cure.  The cured compound is an outstanding electrical insulator.  EP41S Medical’s low viscosity makes it excellent for small encapsulations, pottings and castings.  In addition, EP41S Medical meets USP Class VI specifications, making it well suited for a variety of uses in medical devices as an adhesive, sealant and coating.  EP41S Medical also meets FDA requirements listed above for food compatibility.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2009 Master Bond Inc., All Rights Reserved