LTX119 Product Description

High Performance, Pressure Sensitive, UV StableVinyl Acrylic/Adhesive Latex

Master Bond Polymer System LTX119 is a high performance vinyl acrylic latex with aggressive peel and tack for many industrial pressure sensitive adhesive applications. This product, with its superior UV stability and excellent oxidation resistance, its low skin irritation properties and low odor level, adheres well to a wide variety of both ridge and flexible substrates. Adhesions to polyethylene's, polypropylenes, polyesters, and cellulosies is excellent. Master Bond Polymer System LTX119 also exhibits very superior adhesion to spun bonded polyolefins such as Tyvek. It conforms compositionally with FDA Regulation 175.105.

LATEST PRODUCT

Offering a unique blend of high performance properties, Master Bond MasterSil 153 is often used in a...

LATEST WHITE PAPER

Selecting the right adhesive is a balancing act as engineers attempt to find products that meet conflicting end-use and...