High Performance, Pressure Sensitive, UV Stable Acrylic Adhesive Latex

Master Bond Polymer System LTX162 is a high performance acrylic latex with aggressive peel and tack for many industrial pressure sensitive adhesive applications. This product, with its superior UV stability and excellent oxidation resistance, its low skin irritation properties and low odor level, adheres well to a wide variety of both rigid and flexible substrates.