LTX165 Product Description

High Performance, Extremely Versatile, Pressure Sensitive, Acrylic Co-Polymer Latex Adhesive, Aggressive Dry Tack, Formulated For Bonding Polyolefins and Difficult to Bond Substrates

Master Bond Polymer System LTX 165 is a pressure sensitive high performance acrylic co-polymer emulsion. It features a combination of flexibility, excellent toughness, and durability. Master Bond Polymer System LTX165 can be applied over porous as well as nonporous surfaces. LTX165 dries with excellent clarity, complies with FDA Regulations concerning Food Packaging Adhesives/FDA Status 21 CFR 175.105 and 21 CFR 175.125.

LATEST PRODUCT

Offering a unique blend of high performance properties, Master Bond MasterSil 153 is often used in a...

LATEST WHITE PAPER

Selecting the right adhesive is a balancing act as engineers attempt to find products that meet conflicting end-use and...