High Performance Acrylic Polymer Based, Pressure Sensitive Hot Melt With Excellent Adhesion To Metals, Glass, Plastics, Paper, Fabrics, And Other Substrates

Master Bond Polymer System MB528 is a high performance 100% solid acrylic resin based hot melt compound designed for use as a hot melt pressure sensitive adhesive. It exhibits good adhesion to a wide variety of materials including polyester, glass, aluminum, steel, fabric and paper. Master Bond MB528 provides a medium degree of cohesive strength with good resistance to creep or cold flow. MB528 is a thermoplastic acrylic resin which can be applied using a variety of hot melt coating equipment. This resin may be used as is, or modified with compatible plasticizers, such as resin based, hydrocarbon, or terpene-phenolic resins.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2008 Master Bond Inc., All Rights Reserved