Master Bond Polymer System MB602 is a one component latex based high performance adhesive composition for temporary bonding applications to glass, ceramics, metals, wood, papers, celluloses and other plastics. Most adhesives presently available for temporary bonding usage such as waxes, hot melts, and various organic solvent compounds often lack desirable properties such as dimensional stability and ease of application. They can also sometimes present health and environmental issues. Finally these temporary adhesives are difficult to completely remove without leaving some degree of residual surface contamination. Master Bond Polymer System MB602 is a newly developed single component cost effective temporary adhesive composition which overcomes the current deficiencies of the presently employed temporary adhesives. MB602 is easily removed by water, particulary warm or hot water.
|