Master Bond MasterSil 154 Product Description

 

MASTER BOND MASTERSIL 154
Two Component, Electrically Conductive Silicone Compound For High Performance
Bonding And Sealing Cures To A Tough Flexible Electrical Conductive Clear Rubber Featuring Low Electrical Resistance

Master Bond MasterSil 154 is a two component tan colored electrically conductive silicone compound for high performance bonding and sealing. The specifically modified silicone resin after the addition of a liquid curing agent cures at ambient or more quickly at elevated temperatures to a tough, flexible, electrically conductive silicone rubber. The tightly controlled viscosity of this silicone elastomer compound produces a smooth paste which assures complete fill-in around complicated contours in even very complex configurations and provides excellent electrical conductivity as well as superior resistance to vibration and shock after cure. It has been widely accepted for bonding and/or sealing of electronic components, electrical devices and various electrooptical systems as well for special electronic circuitry or wherever a tough, elastic electrically conductive adhesive or sealant offering superior protection against adverse environmental conditions is required. Master Sil 154 is silver filled and has outstanding conductivity properties.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2008 Master Bond Inc., All Rights Reserved