Master SIL 713 Product Description

 

MASTER SIL 713
One Component, Room Temperature Curing, Silicone Elastomer Compound For High Performance Bonding and Sealing Featuring Exceptionally Low Viscosity

Master Sil 713 is a ready-to use, exceptionally low viscosity, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This compound is self leveling and can be readily applied to various surfaces. It cures at ambient temperatures to a flexible rubbery solid when exposed to atmospheric moisture. Master Sil 713 is an excellent electrical insulator and provides vibration and shock protection for delicate electronic components. It remains flexible and provides excellent service over the broad temperature range of -75°F (-60°C) to +400°F (205°C). Color is clear. Master Sil 713 silicone adhesive/sealant is widely employed for its reliable and high quality performance for bonding, sealing and joining metal, plastics, electrical insulations, protective coatings, formed-in-place gaskets and encapsulation of sensitive electronic components. This product can also be employed as a solventless conformal casting.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2009 Master Bond Inc., All Rights Reserved