Master Bond Polymer System MasterSil#726 Product Description
MASTER BOND POLYMER SYSTEM MASTERSIL#726
Non-Curing Thermally, Conductive Silicone Compound for Heat Transfer Applications.
Master Bond Polymer System MasterSil#726 is a non-curing grease-like thermally conductive silicone compound. It is extremely stable, it will not dry out, cure, harden, or bleed, even after exposure to temperatures as high as 200C (392F). MS#726 is used on transistors, diodes, rectifiers and transformers to dissipate heat and to increase performance life of electrical components.