Master Bond Polymer Adhesive SUPREME 10AOHT represents a breakthrough in epoxy adhesive
technology featuring a thus far unattainable balance of performance properties including both high shear
and high peel strength. It exhibits high thermal conductivity and excellent electrical insulation properties.
This one component adhesive system is formulated to cure at elevated temperatures e.g. 1 hour at 250°-
300°F. Tensile lap shear strength is 1500 psi. No mixing is necessary prior to use. Master Bond Polymer
Adhesive SUPREME 10AOHT produces good bonds with both high shear and high peel strength for
service in the remarkably wide temperature range of 4K to 400°F. It offers very superior resistance to
impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep,
corrosion and thermal resistance typical of epoxy resin adhesives. It is 100% reactive and does not
contain any diluents or solvents.
Master Bond Polymer Adhesive SUPREME 10AOHT produces durable high strength, thermally
conductive, exceptionally tough bonds which are remarkably resistant to severe thermal cycling and many
chemicals including water, oil, fuels and most organic solvents even upon prolonged exposures.
Adhesion to metals, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. The
hardened adhesive is a superior thermal conductor. Color is gray. Master Bond Polymer Adhesive
SUPREME10AOHT offers the convenience of a heat cure with no mixing prior to use and a uniquely
favorable bonding performance for even the most difficult applications in the aerospace, electronic,
electrical, computer, metalworking, appliance, automotive and chemical industries. |