Go to the MasterBond.com home page
Master Bond Polymer System UV10 MEDICAL Product Description

 

MASTER BOND POLYMER SYSTEM UV10 MEDICAL
One Component, Optically Clear, USP Class VI Approved, UV Curable
Compound With Extended Service Capability of -60°F to +250°F
For High Performance Bonding, Sealing and Coating.

Master Bond UV10 Medical is a one component, UV curable system that fully meets USP Class VI specifications. This low viscosity, optically clear system is a superior adhesive, sealant and coating and is castable beyond 1/8" thick. The cured system has good chemical resistant properties particularly to sterilants. It has excellent adhesion to a wide variety of substrates, particularly glass and optically clear plastics. The electrical insulation properties of UV10 Medical are superior to many other UV systems. Service temperature range is -60 to 250°F.

Unlike some other UV curable products, the low viscosity Master Bond UV10 Medical is not inhibited by air and exhibits a desirable fast curing rate at ambient temperatures even at section thickness greater than 1/16". Cure time depends on the type of UV lamp, the wave lengths and the amounts of the emitted UV radiation, distance of the lamp from the top surface of the UV10 Medical, the thickness of the section to be cured, etc. Typical cure times range from as little as 5-10 seconds to 2-3 minutes at ambient temperatures. 200 watt/inch medium pressure mercury vapor lamps or equivalent UV light sources are recommended. Maximum UV absorption takes place in the 280-360 nanometer range. No solvents or other vapors are released during the curing process which takes place with minimal shrinkage from the liquid to the solid state. The storage stability of the UV10 Medical system is 3 months under usual storage conditions e.g. 70°F, in original, unopened containers. The performance profile of the UV10 Medical system makes it highly desirable for many medical device manufacturing applications.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2008 Master Bond Inc., All Rights Reserved