Go to the MasterBond.com home page
Master Bond Polymer System UV15X-6MED-2 Product Description

 

MASTER BOND POLYMER SYSTEM UV15X-6MED-2

One Component High Viscosity UV Curable System For Bonding, Sealing, Coating
and Casting Featuring High Flexibility and Outstanding Abrasion Resistance
Fully meets USP Class VI Specifications for Medical Applications, Optical Clarity

Master Bond Polymer System UV15X-6MED-2 is a newly developed one component clear, non‑yellowing, UV curable urethane elastomer system possessing high flexibility and outstanding abrasion resistance.  This high viscosity system can be used for bonding, sealing, coating and casting.  Master Bond UV15X-6MED-2 offers excellent physical strength properties including high elongation, superb resistance to severe environmental conditions as well as the ability to withstand thermal cycling and thermal and mechanical shock.  The service temperature range is ‑80°F to +300°F.  UV15X-6MED-2 bonds well to a variety of substrates including glass, various plastics such as polycarbonates and acrylics, selected rubbers, and metals.  In addition, Master Bond UV15X-6MED-2 possesses excellent thermal and electrical insulation properties.  UV15X-6MED-2 is 100% reactive and does not contain solvents or other volatiles. Most importantly, UV15X-6MED-2 meets USP Class VI specifications.

With commercially available UV lamps cures “on demand” can be effected in very short time periods i.e. 1 minute or less at ambient temperatures.  For example, when curing the UV15X-6MED-2 in thinner sections (10 mils or less) with a 200 watt mercury vapor continuous light source emitting at 365 nm, UV15X-6MED will cure tack free within 10 seconds at 40 milliwatts of output per cm².  UV15X-6MED-2 will cure in thickness greater than 1/8” thick although the cure is not quite as rapid as it would be in thinner sections.

Master Bond Polymer System UV15X-6MED-2 is not air inhibited.  No solvents or other volatiles are emitted during cure.  Master Bond UV15X-6MED-2 contains an exceptionally active UV curing initiator which makes cures practical even with relatively low intensity UV light sources.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2009 Master Bond Inc., All Rights Reserved