High Performance Elastomer Based One-Component Adhesive For Fast
Durable Bonding and Sealing of Polyolefins Without Surface Pretreatment.
Also Functions as Polyolefinic Primer.

Master Bond Polymer System X17 is a specially formulated one component adhesive especially designed for bonding polyolefins such as polypropylene, polyethylene as well as their many co-polymers and blends. This synthetic elastomer based adhesive compound exhibits a unique balance of both shear and peel properties when bonding polyolefin substrates to each other, as well as to related substrates including flexible PVC. Master Bond Polymer Systems X17 contains 30% solids and has a carefully formulated solvent blend which readily evaporates as cure proceeds. X17 works best when surfaces are mated immediately after the application of adhesive to each substrate. An initial set occurs readily in Master Bond X17 upon evaporation of less than 25% of the solvent. The strength of this initial set usually suffices to maintain the assembly in position for handling. Bond strength increases sharply as evaporation of the solvent progresses and with some adherents it might approach the strength of the substrate materials. Maximum bond strength is obtained upon complete evaporation of the solvent. Optimal performance bonds can be obtained at ambient temperatures within 12-24 hours. Although adding heat is not obligatory for curing, application of heat (120°F-180°F) will greatly accelerate the rate of cure and also increase final bond strengths significantly. All substrates should be free of grease, dirt, oil and other contaminants for best results. Conventional cleaning methods such as solvent washing and vapor degreasing are recommended for maximum bond strength. This product is also an effective primer for polyolefin surfaces such as polyethylene and polypropylene in conjunction with adhesives such as epoxies, urethanes, etc.

Master Bond Polymer System X17 is a readily flowable clear liquid. It can be further thinned with ketone and aromatic solvents. Cured Master Bond Polymer X17 adhesive retains its outstanding strength properties even after prolonged exposure to water and many other chemicals including alcohols and aliphatic hydrocarbons. Cross hatch tape adhesion tests have given outstanding results after merely air dry curing methods. Master Bond Polymer System X17 offers a simple to use, technically effective solution to the problem of bonding polyolefin substrates. It represents a major advance in the formulation of high performance polyolefin bonding systems. Since Master Bond X17 contains volatile solvents it must be employed in a ventilated area taking all necessary precautions for handling adhesive materials comprising of volatiles.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2008 Master Bond Inc., All Rights Reserved