News Releases

Stay informed about Master Bond's latest product developments, company events, and other exciting announcements.
 

Release Date:
Product: EP21ARHT

Developed for coating and lining storage tanks, piping, scrubbers, and processing equipment in the chemical industry, Master Bond EP21ARHT features outstanding chemical, fuel, and acid resistance. Also widely used in electronic, electrical, and metalworking industries, it can even successfully withstand immersion to 96-98%…

Release Date:
Product: EP65HT-1

Master Bond EP65HT-1 combines high temperature resistance and fast room temperature curing in a NASA low outgassing approved epoxy. It also offers superior electrical insulation capabilities and strong chemical resistance.

With an extremely high glass transition temperature exceeding 125ºC, EP65HT-1 features fast cure…

Release Date:
Product: EP30D-7

Combining the benefits of epoxy resins and polyurethanes, Master Bond Polymer System EP30D-7 offers superior strength, flexibility, abrasion resistance and toughness. This two component epoxy is ideal for high performance bonding, sealing, coating, and encapsulating applications in the electronic, electrical, computer,…

Release Date:
Product: EP30FLAO

Master Bond EP30FLAO is a two component epoxy resin system for high performance potting, bonding, sealing and coating. It is extremely versatile and can be used in a wide variety of cryogenic applications. This low viscosity epoxy with excellent flow characteristics makes it ideal as a thermally conductive potting compound. It…

Release Date:
Product: EP31

For superb adherence to a wide variety of substrates including many metals, plastics, rubbers, ceramics and glass, Polymer System EP31 was developed by Master Bond Inc. This two part system features extraordinary adhesion with a lap shear strength exceeding 4,600 psi, a peel strength surpassing 40 pli, a tensile modulus of more…