EP39-2
Two component, low viscosity, room temperature curing epoxy for bonding, sealing, coating and casting
Key Features
- Serviceable up to 300°F
- Superior chemical resistance
- Exceptional optical clarity
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
2,000-4,000 cps
Cure Schedule
3-4 hours at ambient temperatures followed by 2-3 hours at 140-170°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +300°F
Dielectric Constant
4.3
Refractive Index
1.55
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
1,000 Hours at 85°C/85% RH
Case Study
EP39-2: Used as a photoelectrode encapsulant in photoelectrochemical (PEC) system for hydrogen production
University of Hawaii researchers, under the sponsorship of the Department of Energy, were looking to develop photoelectrochemical (PEC) systems to produce hydrogen directly from water using sunlight as the energy source. These PEC systems need to be …