EP51HT

Highlight

Two Component, Room Temperature Curing Epoxy Adhesive Featuring Superior and Cost Effective Bonding Performance with Exceptionally Fast Cures for Service from 4K to 400°F.

Typical Properties
Viscosity
60,000-70,000 cps
Cure Schedule
3 hours at 75°F
Service Temperature Range
4K to +400°F
Tensile Lap Shear Strength
3,010 psi
Bild
EP51HT Two Part Epoxy
Applications
Product Description

Master Bond EP51HT represents a significant advance in epoxy adhesive technology featuring an excellent balance of performance properties, including convenient curing at ambient temperatures, and superior cost effective bonding performance for service from 4K to 400°F. This two component adhesive system is formulated to cure exceptionally fast (5 minute gels) at ambient temperatures or even more rapidly at elevated temperatures, with a convenient one to one mix ratio. EP51HT produces exceptionally good performance bonds with high shear strength, for service over a wide temperature range of 4K to as high as 400°F. It offers truly remarkable resistance to impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep, corrosion and thermal resistance desired for high performance and heat resistant bonding. EP51HT is easily mixed and can be applied without sagging or dripping even on vertical surfaces. It is 100% reactive and does not contain any solvents or diluents.

EP51HT produces durable, high strength, exceptionally tough bonds which are remarkably resistant to severe thermal cycling and many chemicals including water, oil, fuels and most organic solvents even upon prolonged exposure at elevated temperatures. Tensile lap shear strengths as high as 3,000 psi are obtained after room temperature cure only and the bonds retain high strength properties when exposed to the 350-400°F range. Adhesion to metals, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. The hardened adhesive is an electrical insulator. Color of Part A is clear, Part B is tan. EP51HT offers the convenience of a room temperature cure with a uniquely favorable balance of performance properties for use in even the most demanding applications in the aerospace, electronic, electrical, computer, construction, appliance, automotive and chemical industries for service up to 400°F.

Product Advantages

  • Convenient mixing: non-critical one to one mixing ratio, by weight.
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly.
  • No-drip formula available (EP51HTND).
  • Versatile cure schedules: exceptionally fast ambient temperature cure or high speed elevated temperature cures as required.
  • High bonding strength to similar and dissimilar substrates over the remarkably wide temperature range of 4K to +400°F.
  • Good electrical insulating properties and chemical resistance.
  • Superior thermal shock, impact and stress cracking fatigue resistance.
  • Excellent long term durability and dimensional stability.
    Show More

    How to order

    Verify Your Product Selection

    With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

    Get a Quote

    Our customer service team will follow up with a detailed quote with packaging and shipping options.

    Place Your Order

    We'll work with your company to process the order efficiently.

    Receive Your Material

    Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.