Supreme 30

Highlight

Low Viscosity, Toughened Two Component Epoxy Adhesive For High Performance General Purpose Bonding.

Typical Properties
Viscosity
Part A: approx 1500 cps at 25°C, Part B: 300-500 cps at 25°C
Cure Schedule
room temp: 85% of maximum strength developed within 24-48 hours; elevated at 40°C (104°F): 16-24 hours; elevated at 100°C (212°F): 2-6 hours
Linear Shrinkage
0.0007 inches/in.
Volume Resistivity
>20 ohm cm at 75°F
Bild
Supreme 30 Two Component Epoxy
Applications
Product Description

Master Bond Polymer Adhesive Supreme 30 is a low viscosity, toughened two component epoxy adhesive for general purpose bonding formulated to cure at room temperature or more rapidly at elevated temperatures, with a four (4) to one (1) mix ratio by weight. This adhesive is 100% reactive and does not contain any solvents or other volatiles. It is especially recommended where low viscosity is required for ease of application and bonding assemblies must exhibit superior dimensional stability. Shrinkage after ambient temperature cure is exceptionally low-0.0007 inches/in.

Master Bond Polymer Adhesive Supreme 30 produces high strength and tough bonds which are remarkably resistant to thermal cycling and chemicals including water, oil and most organic solvents, over the exceptionally wide temperature range of -60°F to more than 250°F. Adhesion to both similar and dissimilar materials including metals, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. The hardened adhesive is an excellent electrical insulator. Color of part A is light amber, part B slightly yellow. Master Bond Polymer Adhesive Supreme 30 is widely used in the electronic, electrical, computer, construction, metalworking, appliance, automotive and chemical industries.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.