EP30M4
Two component epoxy system for high performance applications
Key Features
- bonding, sealing, encapsulation
- Superior chemical resistance
- Curable at ambient or slightly elevated temperatures
- Excellent bond strength
- Moderate viscosity
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 350-700 cps
Cure Schedule
overnight at 75°F followed by a few hours at 150-200°F
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +300°F
Coefficient of Thermal Expansion
45-50 x 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁴ ohm-cm
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
1,000 Hours at 85°C/85% RH
Meets EU Directive 2015/863
Packaging