Supreme 34AO
Toughened, two component epoxy for bonding, sealing and coating
Key Features
- Convenient handling
- Good temperature resistance
- Can withstand thermal cycling
- Thermally conductive & electrically insulative
Typical Properties
Viscosity
Part A: paste, Part B: paste
Cure Schedule
overnight at 75°F followed by 2-4 hours at 150-200°F
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +425°F
Coefficient of Thermal Expansion
30-35 x 10⁻⁶ in/in/°C
Dielectric Constant
4.7
Linear Shrinkage
<0.1%
Tensile Lap Shear Strength
1,600-1,800 psi
Tensile Modulus
400,000-450,000 psi
Thermal Conductivity
9-10 BTU•in/(ft²•hr•°F) [1.30-1.44 W/(m•K)]
Volume Resistivity
>10¹⁴ ohm-cm