Supreme 121AO
Two part toughened epoxy for bonding, sealing and encapsulation features good thermal conductivity
Key Features
- Free flowing viscosity
- High temperature resistance
- Exceptionally long open time
- Passes NASA low outgassing
Typical Properties
Viscosity
10,000-25,000 cps
Cure Schedule
1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties.
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +550°F
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F)
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
Packaging