Supreme 45HT-3
Two component, quartz filled epoxy system for bonding, sealing and casting
Key Features
- Very long open time
- High temperature resistance
- Exceptional compressive strength
- Withstands abrasive forces
Typical Properties
Viscosity
50,000-100,000 cps
Cure Schedule
250°F for 6 to 8 hours, or 4 to 6 hours at 350°F; optimal cure schedule is 300°F for 2 to 3 hours, followed by a post cure at 350°F for 4 to 6 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +550°F
Dielectric Constant
4.5
Glass Transition Temperature (Tg)
145-155°C
Tensile Modulus
550,000-600,000 psi
Volume Resistivity
>10¹⁴ ohm-cm