Supreme 11HTLV
Toughened, high temperature resistant, two component epoxy for bonding, sealing and coating
Key Features
- Convenient handling
- Good shear and peel bond strength
- Withstands thermal cycling
- Low modulus
Typical Properties
Viscosity
Part A: 25,000-35,000 cps, Part B: 2,000-6,000 cps
Cure Schedule
overnight at 75°F, followed by 30 to 60 minutes at 150°F
Hardness
55-65 Shore D
Service Temperature Range
-100°F to +350°F
Coefficient of Thermal Expansion
55-60 X 10⁻⁶ in/in/°C
Tensile Modulus
40,000-50,000 psi
Bild