Fast Curing, Silver Filled Epoxy Meets ISO 10993-5 Cytotoxicity Standards
Master Bond EP77M-FMed is a two part epoxy adhesive and sealant designed for use in the assembly of medical devices. It meets the ISO 10993-5 requirements and is not considered to have a cytotoxic effect. “This product has been formulated to provide excellent electrical and thermal conductivity properties, while keeping in mind processing constraints for heat sensitive components in sensors used for medical devices or wearable electronics,” says Rohit Ramnath, Senior Product Engineer.
As a silver filled system, EP77M-FMed provides excellent electrical conductivity, with a low volume resistivity of 10-3 ohm-cm. It provides a thermal conductivity of 1.44-1.73 W/(m•K), resists thermal cycling and has a Shore D hardness of 40-50 at room temperature. It can withstand exposure to water, liquid sterilants, anti-microbial disinfectants and EtO sterilization. It offers a tensile strength of 2,000-3,000 psi and a tensile modulus of 250,000-300,000 psi at 75°F. This system is serviceable over the temperature range of -100°F to +250°F.
EP77M-FMed has an easy to use one to one mix ratio by weight or volume and is fast setting, especially when compared to other silver filled systems. It sets up in 15-20 minutes at 75°F and fully cures at room temperature in 24 hours. This compound has a flowable paste like consistency and bonds well to a variety of substrates including metals, glass, ceramics, rubbers and many plastics. It is packaged in 20 gram, 50 gram, 100 gram, one pound and multiple pound cans. The color of Parts A and B is silver. EP77M-FMed does not contain any solvents and is RoHS compliant.
For Editorial Use
Click below to download this release in the format of your choice.
| Anhang | Größe |
|---|---|
| EP77M-FMed_nr.doc (27.5 KB) | 27.5 KB |
| Anhang | Größe |
|---|---|
| EP77M-FMed_nr.txt (6.49 KB) | 6.49 KB |
| Anhang | Größe |
|---|---|
| EP77M-F_nr.html (4.14 KB) | 4.14 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.