EP53TC
Two part epoxy with high thermal conductivity, electrically insulating, and low thermal resistance for bonding, sealing, coating, and potting
Key Features
- Applicable in very thin bond lines
- Low thermal resistance
- High thermal conductivity >2.0 W/(m•K)
- Flowable
Typical Properties
Viscosity
45,000-65,000 cps
Cure Schedule
Cures at 80°C for 2 hours followed by 2-4 hours at 90-125°C.
Hardness
85-95 Shore D
Service Temperature Range
-100°F to +300°F
Acoustical Impedance
8.5 MRayl
Thermal Conductivity
16-18 BTU•in/(ft²•hr•°F) [2.31-2.60 W/(m•K)]