Food Grade Certifications

Epoxies that meet FDA CFR 175.105 are designed for indirect and incidental use in food processing equipment. To comply with this specification, every chemical in the formulation must be included on the FDA’s list of approved ingredients, ensuring safety and regulatory alignment.

Epoxies meeting FDA CFR 175.300 represent a higher standard for food grade adhesives than FDA CFR 175.105. They must pass rigorous testing, including extractables limited to less than 0.5 mg/in² after exposure to solvents and elevated temperatures, as well as toxicological evaluations of the cured specimen.

Bild
FDA CFR 175.105

FDA CFR 175.105

Epoxies that meet FDA CFR 175.105 are designed for indirect and incidental use in food processing equipment. To comply with this specification, every chemical in the formulation must be included on the FDA’s list of approved ingredients, ensuring safety and regulatory alignment.
Bild
FDA CFR 175.300

FDA CFR 175.300

Epoxies meeting FDA CFR 175.300 represent a higher standard for food grade adhesives than FDA CFR 175.105. They must pass rigorous testing, including extractables limited to less than 0.5 mg/in2 after exposure to solvents and elevated temperatures, as well as toxicological evaluations of the cured specimen.

Important Note for Using Food Grade Epoxies

When using food grade epoxies, it is important that the end user submit information on all constituents used in the end product to the appropriate agency or organization.

Relevant Content

discuss application

Finden Sie den richtigen Klebstoff für Ihre Anwendung

Mit tausenden Formulierungen bieten unsere erfahrenen Ingenieure eine persönliche Beratung, um sicherzustellen, dass Sie das ideale Material für Ihre spezifischen Anforderungen auswählen.

Möchten Sie sich zunächst selbst umsehen? Entdecken Sie unseren Produktselektor.