Product Selector

Filters
Applications
Product Type
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP110F8-1 Two Part Epoxy
EP110F8-1
Two component, high performance epoxy for potting, sealing, encapsulating and casting
Dielectric Constant
2.81
Elongation
85-95%
  • RoHS Compliant
  • Potting
  • Sealing
  • Encapsulation
  • Casting
  • Bonding
  • Coating
  • Gap Filling
2,500-5,000 cps 4-6 hours at 250-300°F 65-75 Shore D -80°F to +325°F /de/tds/ep110f8-1
EP110F8-3 Two Part Epoxy
EP110F8-3
Two component, high performance epoxy for potting, sealing, encapsulating and casting
Elongation
120-150%
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • Sealing
  • Casting
  • Encapsulation
  • Potting
  • Coating
  • Bonding
  • Gap Filling
1,000-2,000 cps 4-6 hours at 250-300°F 40-50 Shore A -100°F to +300°F /de/tds/ep110f8-3
EP110F8-5 Two Part Epoxy
EP110F8-5
Two component, high performance epoxy for potting, sealing, encapsulating and casting
Coefficient of Thermal Expansion
60-70 in/in X 10⁻⁶/°C
Tensile Modulus
35,000-65,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Potting
  • Sealing
  • Encapsulation
  • Coating
  • Bonding
  • Gap Filling
7,000-11,000 cps 4-6 hours at 250-300°F 70-80 Shore D -100°F to +300°F /de/tds/ep110f8-5
EP112 Two Part Epoxy
EP112
Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation
Refractive Index
1.55
Volume Resistivity
>10¹⁴ ohm-cm
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Impregnation
  • Gap Filling
50-200 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F 75-90 Shore D -60°F to +450°F /de/tds/ep112
EP121CL-LO Two Part Epoxy
EP121CL-LO
Two component epoxy for potting, encapsulation, coating and sealing applications
Dielectric Constant
3.25
Refractive Index
1.56
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Potting
  • Encapsulation
  • Sealing
  • Coating
  • Bonding
1,000-3,000 cps 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F 80-90 Shore D -80°F to +500°F /de/tds/ep121cl-lo
Epoxy System EP125
EP125
Two part epoxy for bonding and sealing featuring very high temperature resistance
Dielectric Constant
3.9
Tensile Lap Shear Strength
2,500-2,700 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
250,000-500,000 cps 3-4 hours at 300°F or 2-3 hours at 350°F 85-95 Shore D -80°F to +600°F /de/tds/ep125
EP126 Two Component Epoxy Compound
EP126
Two part epoxy for bonding and sealing featuring very high temperature resistance
Dissipation Factor
0.091 @ 75F; 0.034 @ 500F
Glass Transition Temperature (Tg)
160 to 180°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
250,000-500,000 cps 3-4 hours at 300°F or 2-3 hours at 350°F -80°F to +600°F /de/tds/ep126
Two Part Epoxy EP126TK
EP126TK
Two part non-drip epoxy for bonding and sealing featuring very high temperature resistance
Dielectric Constant
3.9
Glass Transition Temperature (Tg)
160 to 180°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 3-4 hours at 300°F or 2-3 hours at 350°F; post curing for 12-24 hours at 400-450°F -80°F to +600°F /de/tds/ep126tk
EP21 Two Component Epoxy Compound
EP21
Two component, room temperature curing epoxy compound
Dielectric Constant
2.9
Tensile Lap Shear Strength
2,800-3,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 28,000-42,000 cps, Part B: 45,000-65,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours; Optimum cure schedule: overnight at 75°F, plus 2-3 hours at 150-200°F 70-80 Shore D -60°F to +250°F /de/tds/ep21
EP21AC Epoxy Potting Compound
EP21AC
Two component epoxy system for encapsulating and coating that passes UL746A high amp arc ignition at 3.0 mm thickness with a PLC of 0
Dielectric Constant
2.89 at 9.375 GHz
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • UL 94HB for Flame Retardancy
  • UL 746A for High Amp Arc Ignition Resistance
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Potting
30,000-50,000 cps 75°F: 48-72 hours; 150-175°F: 2-3 hours; Optimal cure: Overnight at 75°F followed by 4-6 hours at 135-165°F 75-85 Shore D -75°F to +194°F /de/tds/ep21ac

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).