EP40ND Two Part Epoxy System
EP40ND
Two component, room temperature curing epoxy with good toughness, paste consistency
Elongation
80-90%
Tensile Lap Shear Strength
1,600-1,800 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 50,000-100,000 cps, Part B: paste overnight at 75°F, followed by a post cure at 120-150°F for 2-3 hours 50-60 Shore D -100°F to +250°F /de/tds/ep40nd
EP40NDMed Two Part Epoxy
EP40NDMed
Two component, medical grade epoxy with good toughness and paste consistency
Elongation
80-90%
Volume Resistivity
>10¹⁵ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 50,000-100,000 cps, Part B: paste overnight at 75°F followed by 2-3 hours at 120°F to 150°F 50-60 Shore D -100°F to +250°F /de/tds/ep40ndmed
Two Part Epoxy EP40TC
EP40TC
Two component, thermally conductive, electrically insulative epoxy system for bonding and sealing
Elongation
60-70%
Tensile Lap Shear Strength
2,300-2,500 psi
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
80,000-100,000 cps overnight at 75°F followed by 3-5 hours at 125°F to 150°F 70-80 Shore D -100°F to +300°F /de/tds/ep40tc
Two Component Epoxy EP40TCMed
EP40TCMed
Two component, thermally conductive, electrically insulative epoxy system for medical device applications
Elongation
60-70%
Tensile Lap Shear Strength
2,300-2,500 psi
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
80,000-100,000 cps overnight at 75°F followed by 3-5 hours at 125°F to 150°F 70-80 Shore D -100°F to +300°F /de/tds/ep40tcmed
EP41S-1 Two Part Epoxy
EP41S-1
Two component, epoxy adhesive, sealant and coating resists harsh chemicals
Dielectric Strength
440 volts/mil
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 10,000-15,000 cps, Part B: 250 - 400 cps 75°F for 24-48 hours, 200°F for 2-3 hours >75 Shore D -60°F to +300°F /de/tds/ep41s-1
EP41S-5 Two Part Epoxy System
EP41S-5
Two component epoxy system featuring excellent chemical resistance especially to solvents, acids, bases, alcohols and fuels
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
140-145°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Casting
  • Encapsulation
  • Gap Filling
25,000-30,000 cps overnight at 75°F followed by 3-4 hours at 150-200°F 85-95 Shore D -80°F to +450°F /tds/ep41s-5
Low viscosity, chemically resistant epoxy system EP41S-5LV
EP41S-5LV
Two component epoxy system featuring excellent chemical resistance especially to solvents, acids, bases, alcohols and fuels
Glass Transition Temperature (Tg)
120-125°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Gap Filling
2,000-5,000 cps 75°F: 3-5 days; 150-200°F: 2-3 hours 85-95 Shore D -80°F to +350°F /tds/ep41s-5lv
Two Part Epoxy EP41S-5Med
EP41S-5Med
Two component epoxy system featuring excellent resistance to sterilants, solvents and autoclaving
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
140-145°C
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
25,000-30,000 cps 75°F: 3-5 days; 150-200°F: 2-3 hours; Optimal cure schedule: overnight at 75°F, plus 3-4 hours at 200°F 85-95 Shore D -80°F to +450°F /tds/ep41s-5med
EP41S-5ND Black Two Part Epoxy
EP41S-5ND Black
Two component epoxy system featuring excellent chemical resistance especially to solvents, acids, bases, alcohols and fuels
Glass Transition Temperature (Tg)
140-145°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
  • Encapsulation
Part A: paste, Part B: paste overnight at 75°F followed by 3-4 hours at 150-200°F 85-95 Shore D -80°F to +450°F /tds/ep41s-5nd-black
EP41S-6
Two component epoxy system that meets UL 1203 for Explosion-Proof and Dust-Ignition-Proof Electrical Equipment for Use in Hazardous (Classified) Locations
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
145-150°C
  • RoHS Compliant
  • UL 1203 for Explosion-Proof & Dust-Ignition-Proof
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Casting
  • Encapsulation
  • Gap Filling
30,000-60,000 cps 24 hours at room temperature followed by 10 hours at 125°C 85-95 Shore D -80°F to +500°F /tds/ep41s-6

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).