Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP21TP-2NV
Two component, epoxy polysulfide for bonding, sealing, coating and encapsulation
Dielectric Constant
3.7
Elongation
40-80%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 4,500-7,500 cps, Part B: 500-3,000 cps 75°F 48-72 hours 40-50 Shore D -80°F to +250°F /de/tds/ep21tp-2nv
EP21TPFL-1 Two Component Epoxy Polysulfide
EP21TPFL-1
Two component, low viscosity epoxy polysulfide for bonding, sealing, coating and casting
Dielectric Constant
3.9
Elongation
>250%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
2,000-4,000 cps Cure at 75°F, 3-5 days 30-50 Shore A -60°F to +250°F /de/tds/ep21tpfl-1
EP21TPFL-1AO Two Part Epoxy Polysuifide System
EP21TPFL-1AO
Flexible two component epoxy polysulfide system for high performance bonding, sealing, coating and potting
Dielectric Constant
4.5
Elongation
150-200%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 15,000-30,000 cps, Part B: 14,000-28,000 cps 75°F, 3-5 days 70-90 Shore A -60°F to +250°F /de/tds/ep21tpfl-1ao
EP21TPHT Two Part Epoxy
EP21TPHT
Two component, epoxy polysulfide for bonding, sealing, coating and encapsulation
Dielectric Constant
3.9
Elongation
20-40%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 90,000-140,000 cps, Part B: 500 - 2,000 cps 48-72 hours at 75°F; optimum cure overnight at 75°F, followed by 2-3 hours at 150°F 55-65 Shore D -80°F to +350°F /de/tds/ep21tpht
Two Part Epoxy EP21TPLV-NV
EP21TPLV-NV
Two component, room temperature curing epoxy polysulfide system
Dielectric Constant
4.1
Elongation
40-80%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 3,000-4,000 cps, Part B: 500-2,000 cps 75°F: 48-72 hours 40-50 Shore D -80°F to +250°F /de/tds/ep21tplv-nv
EP21TPND-NV Two Component Epoxy Polysulfide
EP21TPND-NV
Two component, paste-like epoxy polysulfide for bonding, sealing and coating
Dielectric Constant
3.7
Elongation
20-30%
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 48-72 hours at 75°F 40-50 Shore D -80°F to +250°F /de/tds/ep21tpnd-nv
EP22 Two Part Epoxy Adhesive System
EP22
Aluminum filled, two component epoxy adhesive for bonding, sealing and coating
Coefficient of Thermal Expansion
35-40 in/in X 10⁻⁶/°C
Dielectric Constant
7.5
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 70,000-100,000 cps, Part B: 100,000-150,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours >80 Shore D -60°F to +250°F /de/tds/ep22
EP29LP Two Component Epoxy
EP29LP
Two part, very low viscosity epoxy for bonding, sealing, potting and filament winding
Dielectric Constant
3.9
Dielectric Strength
450 volts/mil
  • RoHS Compliant
  • Bonding
  • Encapsulation
  • Potting
  • Coating
  • Sealing
  • Casting
600-1,700 cps Optimum cure schedule: 75°F for 12-24 hours, followed by a post cure of 4-5 hours at 200°F. >75 Shore D -60°F to +250°F /de/tds/ep29lp
EP29LPAO Two Part Epoxy System
EP29LPAO
Two component, thermally conductive, electrically insulative epoxy system particularly suited for large potting and encapsulation applications
Coefficient of Thermal Expansion
22-24 x 10⁻⁶ in/in/°C
Dielectric Constant
4.4
  • RoHS Compliant
  • Potting
  • Encapsulation
  • Casting
  • Sealing
Part A: 20,000-40,000 cps, Part B: 5,000-15,000 cps EP29LPAO cures at 75°F in 5-7 days or 6-8 hours at 140-180°F. The best cure schedule is overnight at 75°F followed by 4-5 hours at 150°F. 80-90 Shore D -60°F to +250°F /tds/ep29lpao
EP29LPAOHT Two Part Epoxy
EP29LPAOHT
Two component, thermally conductive, electrically insulative epoxy system
Coefficient of Thermal Expansion
22-24 x 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁵ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Potting
  • Coating
  • Bonding
  • Casting
  • Encapsulation
  • Sealing
  • Gap Filling
10,000-30,000 cps overnight at 75°F followed by 4-6 hours at 150°F to 170°F 80-90 Shore D -60°F to +350°F /de/tds/ep29lpaoht