Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
LED405FL One Part LED Curable Adhesive
LED405FL3
One component, flexibilized LED curable system
Refractive Index
1.51
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Casting
  • Encapsulation
500-3,000 cps Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections. 5-15 Shore D -100°F to 250°F /de/tds/led405fl3
LED422DC90 One Part LED and Heat Curing Adhesive
LED422DC90
One component, nanosilica filled dual curing LED system allowing for rapid fixturing and subsequent curing by heat. Complies with NASA low outgassing
Refractive Index
1.49
Tensile Modulus
475,000-575,000 psi
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
2,000-15,000 cps exposure to LED light at 405 nm which induces polymerization in a cross sectional mode, 2-3 mm deep. The cure is then completed by adding heat at 90-95°C for 30-45 minutes. 85-90 Shore D -80°F to +350°F /de/tds/led422dc90
MasterSil 151 Two Part Silicone System
MasterSil 151
Two component, addition curing silicone for potting, encapsulation and sealing
Dielectric Strength
450 volts/mil
Refractive Index
1.436
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
  • Bonding
  • Casting
Part A: 2,000-4,000 cps, Part B: 50-150 cps 75°F 24-48 hours; 200°F 1-2 hours 50-60 Shore A -65°F to +400°F /de/tds/mastersil-151
MasterSil 151Med Black Two Part Medical Grade Silicone
MasterSil 151Med Black
Two component, biocompatible silicone compound for bonding, potting and encapsulation
Dielectric Strength
450 volts/mil
Volume Resistivity
10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Encapsulation
  • Potting
  • Coating
  • Sealing
  • Gap Filling
  • Casting
Part A: 2,000-4,000 cps, Part B: 50-150 cps 75°F: 24-48 hours; 200°F: 1-2 hours 40-50 Shore A -65°F to +400°F /de/tds/mastersil-151med-black
MasterSil 151S Two Part Silicone System
MasterSil 151S
Two part, silver filled, low outgassing silicone for bonding, sealing and coating
Elongation
100-150%
Volume Resistivity
0.004 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: 50-150 cps 4-6 hours at 150 to 180°F and 2-3 hours at 190 to 210°F 80-90 Shore A -80°F to +400°F /de/tds/mastersil-151s
MasterSil 151TC Two Part Silicone
MasterSil 151TC
Two part, room temperature curing, thermally conductive silicone with ultra fine particle filler for bonding and smaller gap filling
Dielectric Strength
450 volts/mil
Thermal Conductivity
4.0-5.8 BTU•in/(ft²•hr•°F)
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Gap Filling
  • Sealing
  • Coating
  • Casting
  • Potting
  • Encapsulation
30,000-60,000 cps Optimum cure is overnight at 75°F followed by 1-2 hours at 150-200°F. 80-90 Shore A -65°F to +400°F /de/tds/mastersil-151tc
MasterSil 153AOMed Two Part Medical Grade Silicone
MasterSil 153AOMed
Two part medical grade, thermally conductive, electrically insulating silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
100-120%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 200,000-550,000 cps, Part B: 100,000-500,000 cps overnight at 75°F followed by 2-4 hours at 135°F to 185°F 65-75 Shore A -65°F to +400°F /de/tds/mastersil-153aomed
MasterSil 153Med Two Part Silicone
MasterSil 153Med
Two component, addition cured medical grade silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
400-500%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 150,000-300,000 cps, Part B: 50,000-250,000 cps 75°F: 48-72 hours 20-35 Shore A -65°F to +400°F /de/tds/mastersil-153med
Two Part Silicone MasterSil 153Med Black
MasterSil 153Med Black
Two component, paste consistency, addition cured medical grade silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
400-500%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 150,000-300,000 cps, Part B: 50,000-250,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours; Optimum cure: Overnight at 75°F followed by 1 hour at 150-200°F 20-35 Shore A -65°F to +400°F /de/tds/mastersil-153med-black
MasterSil 155 Two Part Silicone System
MasterSil 155
Two part, graphite filled silicone for high performance bonding, sealing and coating
Elongation
300-400%
Volume Resistivity
20-40 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 75°F: 6-7 days; 150°F: 2-4 hours; Optimum cure schedule: overnight at 75°F followed by 2-4 hours at 150°F 35-45 Shore A -85°F to +400°F /de/tds/mastersil-155