Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
MB297Med One Part Ethyl Cyanoacrylate Compound
MB297Med
High viscosity ethyl cyanoacrylate for bonding applications for use with medical devices
Tensile Lap Shear Strength
2,410 psi (Brass-Brass)
Volume Resistivity
>10¹⁵ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
2,200-2,400 cps 20-50 seconds depending upon the humidity and the substrates, 75°F 70 Shore D -60°F to +250°F /de/tds/mb297med
MB297Med-1 One Part Ethyl Cyanoacrylate Adhesive
MB297Med-1
Moderate viscosity ethyl cyanoacrylate for medical device bonding applications
Tensile Lap Shear Strength
1,100 psi
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
1,000-1,100 cps Set up time, 75°F 15-45 seconds (substrate dependent) 70 Shore D -60°F to +250°F /de/tds/mb297med-1
MB297Med-2 One Part Ethyl Cyanoacrylate Compound
MB297Med-2
Lower viscosity ethyl cyanoacrylate for medical device bonding applications
Tensile Lap Shear Strength
1,050 psi
Volume Resistivity
>10¹⁵ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
100-110 cps Set up time, 75°F 10-40 seconds (substrate dependent) 70 Shore D -60°F to +250°F /de/tds/mb297med-2
MB297Med-3 Single Component Ethyl cyanoacrylate
MB297Med-3
Very low viscosity ethyl cyanoacrylate for medical device bonding applications
Tensile Lap Shear Strength
1,230 psi (ABS-ABS)
Volume Resistivity
>10¹⁵ ohm-cm
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
10-20 cps Set up time, 75°F 5 to 35-40 seconds (substrate dependent) 70 Shore D -60°F to +250°F /de/tds/mb297med-3
MB600G One Part Sodium Silicate Coating
MB600G
One component, electrically conductive sodium silicate, aqueous based coating system
Specific Gravity
1.53
Surface Resistivity
1-10 ohm
  • RoHS Compliant
  • Coating
Paste 75°F 24-48 hours, 175°F (do not exceed 175°F) 1-2 hours 0°F to +700°F /de/tds/mb600g
MB600S One Part Sodium Silicate System
MB600S
One component, electrically conductive sodium silicate, aqueous based coating system
Specific Gravity
4.4
Surface Resistivity
<1 milliohm
  • RoHS Compliant
  • Coating
Paste 75°F: 24-48 hours; 175°F (do not exceed 175°F): 1-2 hours 0°F to +700°F /de/tds/mb600s
MB600SCN One Part Sodium Silicate Coating
MB600SCN
One component, electrically conductive sodium silicate, aqueous based coating system
Specific Gravity
3.0
Surface Resistivity
<10 milliohm
  • RoHS Compliant
  • Coating
paste 75°F: 24-48 hours; 175°F (do not exceed 175°F): 1-2 hours 0°F to +700°F /tds/mb600scn
Super Gel 9 Two Part Urethane Modified Epoxy
Super Gel 9
Two component urethane modified epoxy gel-like system
Dielectric Strength
>420 volts/mil
Refractive Index
1.5253
  • RoHS Compliant
  • Bonding
  • Sealing
  • Casting
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
3,000-9,000 cps cures at 75°F, 4-7 days <5 Shore A -100°F to +200°F /de/tds/super-gel-9
Supreme 10AOHT One Part Epoxy System
Supreme 10AOHT
One component, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing
Tensile Lap Shear Strength
3,400-3,600 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 250°F for 60-70 minutes, 300°F for 40-50 minutes 80-85 Shore D 4K to +400°F /de/tds/supreme-10aoht
Supreme 10AOHT-LO One Part Epoxy System
Supreme 10AOHT-LO
One component, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing meets NASA low outgassing specifications
Dielectric Constant
4.3
Tensile Lap Shear Strength
3,400-3,600 psi
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
paste 250°F for 60-70 minutes, 300°F for 40-50 minutes 80-90 Shore D 4K to +400°F /de/tds/supreme-10aoht-lo