Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
Supreme 10HT One Part Epoxy
Supreme 10HT
One component, toughened epoxy system
Glass Transition Temperature (Tg)
130-135°C
Tensile Lap Shear Strength
3,600-3,800 psi
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
>500,000 cps 60-75 minutes at 250°F; 35-40 minutes at 300°F 70-80 Shore D 4K to +400°F /de/tds/supreme-10ht
Supreme 10HTCL Single Component Epoxy
Supreme 10HTCL
One component, heat resistant toughened epoxy system passes NASA low outgassing
Tensile Lap Shear Strength
2,800-3,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
140,000-200,000 cps 60-75 minutes at 250°F 70-80 Shore D 4K to +400°F /de/tds/supreme-10htcl
Supreme 10HTF-1 One Part Epoxy Compound
Supreme 10HTF-1
One component, fast curing, toughened epoxy adhesive/sealant
Tensile Lap Shear Strength
>3,200 psi
Tensile Modulus
350,000-400,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
>500,000 cps 5-10 minutes at 300°F or 15-20 minutes at 250°F; post cure at 250-300°F for 1-2 hours >70 Shore D 4K to +400°F /tds/supreme-10htf-1
Supreme 10HTFL One Component Epoxy
Supreme 10HTFL
One component, flexibilized epoxy system
Dielectric Constant
4.5
T-peel Strength
40-50 pli
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
350,000-700,000 cps 20-30 minutes at 300°F or 45-60 minutes at 250°F 45-65 Shore D 4K to +350°F /de/tds/supreme-10htfl
Supreme 10HTLV One Part Epoxy System
Supreme 10HTLV
One component, toughened epoxy system
Tensile Lap Shear Strength
3,600-3,800 psi
Volume Resistivity
>10¹² ohm-cm
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
200,000-400,000 cps 60-75 minutes at 250°F; 35-40 minutes at 300°F 70-80 Shore D 4K to +400°F /de/tds/supreme-10htlv
Supreme 10HTN One Part Epoxy
Supreme 10HTN-NV
One component, heat curing, nickel conductive epoxy system
Tensile Lap Shear Strength
1,200-1,400 psi
Volume Resistivity
5-10 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste minimum 250°F for 60-90 minutes 85-95 Shore D 4K to 400°F /de/tds/supreme-10htn-nv
Supreme 10HTND-3 One Part Epoxy
Supreme 10HTND-3
One component, toughened epoxy system
Tensile Strength
8,000-9,000 psi
Tensile Modulus
450,000-500,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 60-75 minutes at 250°F 75-85 Shore D 4K to +400°F /de/tds/supreme-10htnd-3
Supreme 10HTS One Part Epoxy
Supreme 10HTS
One component, heat curing, toughened epoxy system
Tensile Lap Shear Strength
>1,200 psi
Volume Resistivity
<0.006 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
>500,000 cps 250°F for 60-75 minutes, 300°F for 40-45 minutes >75 Shore D 4K to +400°F /de/tds/supreme-10hts
Supreme 112: two part epoxy for bonding, sealing, potting and impregnation
Supreme 112
Two part epoxy for bonding, sealing, potting and impregnation requires elevated temperature curing
Glass Transition Temperature (Tg)
190-195°C
Volume Resistivity
>10¹⁴ ohm-cm at 25°C, >10¹² ohm-cm at 150°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Impregnation
  • Coating
  • Encapsulation
  • Gap Filling
50-200 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F 75-90 Shore D -80°F to +550°F /de/tds/supreme-112
Supreme 11AOHT Two Part Epoxy
Supreme 11AOHT
Two component thermally conductive, electrically insulative epoxy compound for bonding, coating and sealing
Dielectric Constant
4.6
Tensile Lap Shear Strength
3,200-3,400 psi
  • MIL-STD-883J for Thermal Stability
  • RoHS Compliant
  • Bonding
  • Coating
  • Sealing
  • Gap Filling
Part A: 200,000-300,000 cps, Part B: paste 8-12 hours at 75°F, plus 1-2 hours at 150-200°F 80-85 Shore D -112°F to +400°F /de/tds/supreme-11aoht