Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
Supreme 46HT-2 Two Part Epoxy
Supreme 46HT-2
Toughened, two component epoxy system for bonding, sealing and coating
Dielectric Constant
4.5
T-peel Strength
>10 pli
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
15,000-30,000 cps 250-300°F for 3-4 hours 80-90 Shore D -100°F to +500°F /de/tds/supreme-46ht-2
Supreme 46HT-2ND2 Two Component Epoxy
Supreme 46HT-2ND2
Non-drip, two component epoxy system for bonding, sealing and coating
Tensile Lap Shear Strength
2,800-3,000 psi
Tensile Modulus
350,000-400,000 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 250-300°F for 3-4 hours, followed by a post cure at 350-400°F for 1-2 hours 80-90 Shore D -100°F to +500°F /de/tds/supreme-46ht-2nd2
Supreme 46HTQ Two Component Epoxy
Supreme 46HTQ
Two component epoxy system for bonding, sealing and casting
Dielectric Constant
4.6
Tensile Lap Shear Strength
2,000-2,200 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Casting
  • Coating
  • Gap Filling
  • Encapsulation
  • Potting
10,000-25,000 cps 4-6 hours at 250°F and 3-4 hours at 300°F 85-95 Shore D -60°F to +450°F /de/tds/supreme-46htq
Supreme 62-1 Two Part Epoxy
Supreme 62-1
Two component epoxy resin system featuring excellent temperature and chemical resistance
Dielectric Constant
4.2
Tensile Lap Shear Strength
1,600-1,800 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
15,000-25,000 cps Typical cure schedules range from 4-6 hours at 140-158°F [60-70°C], 20-40 minutes at 176-212°F [80-100°C] or 10-20 minutes at 257°F [125°C] 75-85 Shore D -60°F to +450°F /de/tds/supreme-62-1
Supreme 70CN Two Part Epoxy
Supreme 70CN
Two component, toughened epoxy system for bonding, sealing, coating and potting derived from natural substances
Dielectric Constant
4.5
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
8,000-12,000 cps overnight at 75°F followed by 4-5 hours at 140-170°F 75-85 Shore D -150°F to +400°F /de/tds/supreme-70cn
UV10 One Part UV Curable Compound
UV10
UV curable, very low viscosity adhesive, sealant and coating
Dielectric Constant
3.5
Refractive Index
1.557
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
250-500 cps UV light at 325-365 nm for 20-30 seconds 70-80 Shore D -60°F to +250°F /de/tds/uv10
UV10-FD One Part UV System
UV10-FD
UV curable, very low viscosity adhesive, sealant and coating; contains a flourescent dye for identification
Refractive Index
1.557
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
250-500 cps UV light 325-365 nm for 20-30 seconds 70-80 Shore D -60°F to +250°F /de/tds/uv10-fd
UV10LV One Component UV Curable System
UV10LV
UV curable, very low viscosity adhesive, sealant and coating
Dielectric Constant
3.7
Refractive Index
1.557
  • RoHS Compliant
  • Bonding
150-350 cps 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2 70-80 Shore D -60°F to +250°F /de/tds/uv10lv
UV10Med One Part UV Curable System
UV10Med
UV curable, biocompatible, low viscosity compound
Refractive Index
1.557
Volume Resistivity
>10¹⁴ ohm-cm
  • 1,000 Hours at 85°C/85% RH
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
250-500 cps 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm² 70-80 Shore D -60°F to +250°F /de/tds/uv10med
One component, high viscosity UV curable system UV10TK40M
UV10TK40M
One component, higher viscosity UV curable system for bonding, sealing and coating
Glass Transition Temperature (Tg)
135-140°C
Refractive Index
1.55
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
30,000-60,000 cps cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with 20-40 milliwatts per cm² 75-85 Shore D -60°F to +450°F /de/tds/uv10tk40m