EP21AOND Two Part Epoxy System
EP21AOND
Two component epoxy compound for high performance applications
Dielectric Strength
>400 volts/mil
Tensile Lap Shear Strength
>1,200 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
paste 75°F: 3-4 days; 200°F: 2-3 hours; Optimum cure schedule: overnight at 75°F followed by 3-4 hours at 150-200°F >80 Shore D -60°F to +250°F /tds/ep21aond
EP21AR Two Component Epoxy System
EP21AR
Two part epoxy adhesive, sealant, coating and encapsulating system featuring superb acid resistance
Coefficient of Thermal Expansion
40-45 in/in X 10⁻⁶/°C
Dielectric Strength
440 volts/mil
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 10,000-15,000 cps, Part B: 4,000-6,000 cps 75°F: 24-48 hours; 200°F: 2-3 hours 80-90 Shore D -60°F to +250°F /de/tds/ep21ar
EP21ARHT Two Part Epoxy
EP21ARHT
Two component epoxy adhesive, sealant, coating and encapsulating system
Dielectric Strength
440 volts/mil
Tensile Modulus
400,000-450,000 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 60,000-110,000 cps, Part B: 4,000-6,000 cps 75°F for 24-48 hours, 200°F for 2-3 hours 80-90 Shore D -60°F to +400°F /de/tds/ep21arht
Two Part Epoxy EP21ARHTND-2
EP21ARHTND-2
Two component epoxy adhesive, sealant and coating featuring exceptional resistance to acids
Dielectric Constant
3.8
Tensile Lap Shear Strength
2,200-2,400 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: paste 75°F: 24-48 hours; 200°F: 2-3 hours 75-85 Shore D -60°F to +400°F /de/tds/ep21arhtnd-2
EP21ARLV Two Component Epoxy
EP21ARLV
Two part epoxy adhesive, sealant, coating and encapsulating system featuring low viscosity and superior acid resistance
Dielectric Constant
3.8
Dielectric Strength
440 volts/mil
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 3,000-6,000 cps, Part B: 4,000-6,000 cps overnight at 75°F followed by 4 to 6 hours at 150-200°F 80-90 Shore D -60°F to +250°F /de/tds/ep21arlv
EP21BAS Two Part Radiopaque Epoxy
EP21BAS
Two component, radiopaque epoxy system for bonding, sealing, coating and encapsulation
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
>1,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 75°F: 48-72 hours; 200°F: 2-3 hours >60 Shore D -60°F to +250°F /de/tds/ep21bas
 EP21FL Two Part Epoxy
EP21FL
Toughened, two component epoxy for bonding, sealing and encapsulation
Tensile Modulus
150,000-200,000 psi
Volume Resistivity
10¹⁴ ohm-cm
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
  • Potting
2,000-4,500 cps Optimum cure schedule: overnight at 75°F plus 2-3 hours at 150-200°F 40-50 Shore D -100°F to +250°F /de/tds/ep21fl
EP21FRNS-2 Two Component Epoxy System
EP21FRNS-2
Two component epoxy system for potting, encapsulating and casting
Dielectric Constant
4.5
Tensile Lap Shear Strength
>1,200 psi
  • RoHS Compliant
  • UL 94V-0 Flame Resistant
  • Casting
  • Encapsulation
  • Potting
  • Sealing
Part A: 40,000-70,000 cps, Part B: 30,000-45,000 cps Cures at 75°F, 48-72 hours >75 Shore D -59.8°F to +194°F /de/tds/ep21frns-2
EP21H Two Component, Optically Clear Epoxy
EP21H
Two component epoxy compound for high performance applications
Refractive Index
1.54
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Casting
3,000-6,000 cps 12-24 hours at 75°F, plus 3-4 hours at 150°F >75 Shore D -60°F to +250°F /tds/ep21h
EP21HT Two Part Epoxy System
EP21HT
Two component epoxy compound for high performance applications
Dielectric Constant
2.90
Tensile Lap Shear Strength
>3,000 psi
  • FDA Food Grade 21 CFR 175.105
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 60,000-110,000 cps, Part B: 11,000-15,000 cps Cures within 48-72 hours at 75°F >75 Shore D -60°F to +400°F /de/tds/ep21ht