The following products have recently passed ASTM E595 testing for NASA low outgassing by an independent laboratory. A full list of Master Bond's NASA low outgassing systems is available here.
EP65HT: Easy Handling, Rapid Curing Epoxy Adhesive
image
Ideal for prototyping and manufacturing, EP65HT sets up in just 9-12 minutes at room temperature in 10-20 gram masses. This product allows enough time to adjust part positioning for applications that require more complex fixturing. This two part epoxy has a ten to one mix ratio by weight, but its handling is facilitated by a dispensing gun capable of mixing fast setting materials. This two part epoxy system offers good physical properties, including low shrinkage upon cure, superior dimensional stability, high tensile modulus and superb tensile strength. Its service temperature range operating is -60°F to +400°F [-51°C to +204°C].

For more information, request a technical data sheet on EP65HT
EP46HT-1AO: Thermally Conductive Epoxy Has Glass Transition Temperature of 215°C
image
With exceptional thermal conductivity and electrical insulation properties, EP46HT-1AO is a two component epoxy for high performance bonding and sealing applications. This high temperature resistant system has a glass transition temperature exceeding 215°C. It cures readily with heat and offers a long open time at room temperatures. EP46HT-1AO provides noteworthy dimensional stability, chemical resistance and superior physical strength properties. It also withstands 1,000 hours at 85°C/85% RH.

For more information, request a technical data sheet on EP46HT-1AO
EP17HTND-2: Chemical Resistant, Non-Drip Epoxy Resists Temperatures Up To 650°F
image
EP17HTND-2 is an easy to handle one component epoxy for bonding sealing and coating applications. It has a noteworthy resistance to many chemicals including acids, bases, salts, fuels, oils and many solvents, even at elevated temperatures. This epoxy system features excellent physical properties and a superb electrical insulation profile even at elevated temperatures. EP17HTND-2 is also distinctive in that it has very low exotherm upon curing. Its service temperature range is from -80°F to +650°F [-62°C to +343°C].

For more information, request a technical data sheet on EP17HTND-2
EP36AO: Flexible Epoxy for Potting and Encapsulation Applications
image
B-staged epoxy, EP36AO, features outstanding thermal shock resistance and thermal conductivity over the wide temperature range of -100°F to +500°F [-73.3°C to +260°C]. It is available for use in 30 gram preforms. EP36AO has excellent adhesion to both metallic and non-metallic substrates, plus a high degree of chemical resistance. It also offers exceptional electrical insulation properties.

For more information, request a technical data sheet on EP36AO
UV16: UV Curable System Has Superior Physical Strength and Low Shrinkage
image
UV16 is a one component, high strength, low viscosity UV curable epoxy resin based polymer system for bonding, sealing and coating. It exhibits a desirably fast cure rate at ambient temperature upon exposure to UV light even in the presence of air. This system is also tough, strong and durable. It has excellent bond strength to a wide variety of substrates including plastics, glass, ceramics and most metals. UV16 has a service operating temperature of -80°F to 400°F [-62°C to +204°C]. This cationic curing system has a Tg of 135-140°C after post curing and exhibits outstanding optical clarity.

For more information, request a technical data sheet on UV16

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2016 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.