X21Med: Polyolefin Primer/Adhesive Meets ISO 10993-5 Requirements |
Master Bond X21Med is a one part system that can be used for bonding and priming polyolefinic surfaces. This exceptionally low viscosity (<250 cps) solvent based system is easy to apply and process. It cures tough at room temperature or more rapidly with the addition of heat. X21Med passes ISO 10993-5 tests for cytotoxicity making it suitable for medical device applications.
For more information, request a technical data sheet on X21Med
|
|
X5TC: One Part, Thermally Conductive Elastomer |
Elastomeric adhesive system, X5TC delivers thermal conductivity of 10-12 BTU•in/ft2•hr•°F [1.44-1.73 W/(m•K)] while maintaining excellent electrical insulation properties. It is well suited for bonding dissimilar substrates and performs well when subjected to thermal cycling, vibration, shock and related forces. This system offers solid tensile lap shear and T-peel strength. X5TC has a paste-like consistency and cures at room temperature or more quickly with the addition of heat.
For more information, request a technical data sheet on X5TC
|
| X5SC: One Part Silver Filled Elastomeric System |
X5SC is a solvent based elastomeric system with superb electrical conductivity. This allows it to be utilized not only as an adhesive, but also as a highly effective system for shielding. It has a paste-like consistency and is very easy to use. This system is well suited for bonding dissimilar substrates and performs well when subjected to thermal cycling, vibration, shock and related forces. It also possesses superior thermally conductive properties.
For more information, request a technical data sheet on X5SC
|
| X18: Low Viscosity System for Bonding and Priming Polyolefins |
One component X18 is a specialty system that can be used an adhesive between two polyolefin surfaces or as a primer to promote adhesion for a polyolefin and another type of substrate, such as metals, ceramics, composites and other kinds of plastics. Surfaces primed with X18 are compatible with a wide variety of adhesives. It has a low viscosity of (<2,500 cps) and is easy to apply. X18 can be cured at room temperature or more rapidly at elevated temperatures.
For more information, request a technical data sheet on X18
|
|
|
|